0086 13810327080
Ore: Molybdenum
Capacity: 1000-3000TPD
Process: One-stage open-circuit crushing - two-stage grinding and classification - prioritized flotation and separating tungsten from flotation tailings - tailings disposal
Ore: Tungsten
Capacity: <300TPD
Process: Crushing - grinding, gravity separation - classification, gravity separation - tailings dry stacking
Ore: Phosphorite
Capacity: 300-1000TPD
Process: Desliming - one-stage closed-circuit grinding - direct flotation process of one-stage roughing, one-stage scavenging and two-stage concentration - concentrates and tailings dewatering
Ore: Graphite
Capacity: 300-1000TPD
Process: Two-stage closed-circuit crushing - one-stage closed-circuit grinding and classification - flotation process of one-stage roughing, two-stage scavenging and ten-stage concentration
Ore: Feldspar
Capacity: 300-1000TPD
Process: Two-stage closed-circuit crushing and screening - one-stage closed-circuit grinding and classification - magnetic separation, desliming and indirect flotation - mechanical dewatering
Ore: Fluorite
Capacity: 300-1000TPD
Process: Two-stage closed-circuit crushing - one-stage closed-circuit grinding and classification - flotation process of one-stage roughing, one-stage scavenging and seven-stage concentration - concentrates and tailings dewatering - concentrates drying
Ore: Multi-Metal
Capacity: 3000-6000TPD
Process: Two-stage continuous grinding - flotation - comprehensive concentrate regrinding – two-stage leaching and two-stage washing - zinc powder displacement process.
Ore: Molybdenum
Capacity: 1000-3000TPD
Process: Two stage one closed circuit crushing and screening-three stage closed circuit grinding-flotation (one roughing, two scavenging and seven cleaning + two fine scavenging) - concentrate dehydration process.