0086 13810327080
Ore: Gold
Capacity: 300-1000TPD
Process: One-stage open-circuit crushing and classification - one-stage open-stage self-grinding - one-stage closed-circuit grinding and classification - flotation - concentrates dewatering
Ore: Iron
Capacity: 1000-3000TPD
Process: Two-stage closed-circuit crushing and screening - two-stage closed-circuit grinding and classification - magnetic separation process of one-stage roughing and three-stage concentration - concentrates and tailings filtering and dewatering
Ore: Molybdenum
Capacity: 1000-3000TPD
Process: One-stage open-circuit crushing - two-stage grinding and classification - prioritized flotation and separating tungsten from flotation tailings - tailings disposal
Ore: Feldspar
Capacity: 300-1000TPD
Process: Two-stage closed-circuit crushing and screening - one-stage closed-circuit grinding and classification - magnetic separation, desliming and indirect flotation - mechanical dewatering
Ore: Fluorite
Capacity: 300-1000TPD
Process: Two-stage closed-circuit crushing - one-stage closed-circuit grinding and classification - flotation process of one-stage roughing, one-stage scavenging and seven-stage concentration - concentrates and tailings dewatering - concentrates drying
Ore: Multi-Metal
Capacity: 3000-6000TPD
Process: Two-stage continuous grinding - flotation - comprehensive concentrate regrinding – two-stage leaching and two-stage washing - zinc powder displacement process.
Ore: Molybdenum
Capacity: 1000-3000TPD
Process: Two stage one closed circuit crushing and screening-three stage closed circuit grinding-flotation (one roughing, two scavenging and seven cleaning + two fine scavenging) - concentrate dehydration process.
Ore: Gold
Capacity: 300-1000TPD
Process: Two-stage a closed circuit crushing and screening – two-stage closed circuit grinding - flotation (two-stage roughing, two-stage scavenging and three-stage concentration) – concentrate and tailings dewatering.
Ore: Feldspar
Capacity: 300-1000TPD
Process: Two-stage semi-closed-circuit crushing and screening process---One stage closed-circuit grinding and classifying process---One roughing three concentration three sweeping flotation process---Concentrate tailings conveying process
Ore: Lead-Zinc
Capacity: 1000-3000TPD
Process: Two-and-half-stage and one closed-circuit crushing and screening-One stage of grinding and grading-Flotation- Concentrated tailings dehydration process.
Ore: Tailings
Capacity: 1000-3000TPD
Process: The dehydration process of hydrocyclone + dehydration screen + filter press.
Ore: Phosphorite
Capacity: 1000-3000TPD
Process: Pre-screening and one-stage open-circuit crushing--one-stage grinding--three-stage reverse flotation--phosphate concentrate concentration and dewatering process.
Ore: Lead-Zinc
Capacity: 1000-3000TPD
Process: Two-and-half-stage and one closed-circuit crushing and screening+First closed-circuit grinding+ Zinc-sulfur bulk flotation+ Zinc-sulfur separation flotation+ Concentrate dehydration + Tailings dehydration process.
Ore: Lead-Zinc
Capacity: 1000-3000TPD
Process: Two and half stage closed-circuit crushing and screening – Three stage closed-circuit grinding- Lead flotation- Zinc flotation- Sulfur flotation-lead and zinc concentrate dewatering.
Ore: Multi-Metal
Capacity: 1000-3000TPD
Process: Three stage and one closed circuit crushing and screening – two stage closed circuit grinding – SO2 manganese leaching - cyanidation leaching silver in full wet process.
Ore: Fluorite
Capacity: 300-1000TPD
Process: Two-stage and one closed-circuit crushing and screening-First full closed-circuit grinding(first grinding+second grading)-Desulfurization flotation-Fluorite flotation (one-roughing, two-scavenging, eight-concentration+concentration I re-grinding closed-circuit)-concentrate dehydration process.
Ore: Iron
Capacity: 300-1000TPD
Process: Stage grinding (two-stage grinding) - stage separation (six-stage magnetic separation) - iron concentrates dehydration - gravity separation from magnetically separated tailings-regrinding - flotation separation process of sulfur and titanium.
Ore: Quartz Sand
Capacity: 1000-3000TPD
Process: Two-stage and one-half closed-circuit crushing and screening--one-stage closed-circuit grinding--desliming--magnetic separation--concentrate dwatering process.
Ore: Phosphorite
Capacity: 300-1000TPD
Process: Two-stage and one closed-circuit crushing and screening - two-stage closed-circuit grinding - decarbonization flotation - one-roughing, one-scavenging, one-concentration positive flotation - one-roughing, two-scavenging reverse flotation + one-roughing, one-scavenging, one-concentration sulfur flotation - fine tailings dehydration process.
Ore: Gold
Capacity: 300-1000TPD
Process: Thickener + filter press for gold dewatering process.
Ore: Lead-Zinc
Capacity: 300-1000TPD
Process: Two-and-half-stage and one closed-circuit crushing and screening - one-stage closed-circuit grinding - lead flotation(one-roughing, two-scavenging, three-concentration) - zinc flotation(one-roughing, three-scavenging, two-concentration) - lead and zinc concentrate dehydration process.
Ore: Gold
Capacity: 300-1000TPD
Process: It used the process of one-roughing, three-scavenging, four-concentration for flotation
Ore: Lead-Zinc
Capacity: 300-1000TPD
Process: Differential flotation process (zinc inhibition first and lead flotation then).
Ore: Gold
Capacity: 300-1000TPD
Process: All-slime cyanidation+ CIP process of flotation concentrate. The original 250tpd all-slime cyanidation system was retained, and the new 300tpd grinding and floating system are added. After the thickening, filtration and reagent removal, the flotation concentrate entered into the original 250tpd two-stage grinding mill for regrinding and then entered into the original cyanidation system.
Ore: Copper
Capacity: 3000-6000TPD
Process: Flotation process (one-stage roughing, two-stage scavenging and three-stage concentration).
Ore: Iron
Capacity: 3000-6000TPD
Process: Full closed circuit of three-stage grinding and six-stage separation-concentrates dewatering-tailings dewatering
Ore: Tailings
Capacity: 3000TPD
Process: Flotation tailings adopted dewatering cyclone-dewatering screen-thickener-filter press.
Ore: Iron
Capacity: 1000-3000TPD
Process: Full closed circuit of one-stage grinding and two-stage classification-four-stage magnetic separation-concentrates dewatering-tailings dewatering
Ore: Gold
Capacity: 1000-3000TPD
Process: Crushing – grinding & classification - cyanide leaching - dehydration washing - recovery of cuprous sulfide from filtrate - recovery of gypsum - recovery of hydrogen cyanide gas - gold-containing liquid adsorption, desorption electrolysis, smelting.
Ore: Gold
Capacity: <300TPD
Process: Two stage and one closed circuit crushing - one stage closed circuit grinding and classification - gravity separation and flotation - concentrate tailings dewatering process.
Ore: Gold
Capacity: <300TPD
Process: Two stage and one closed circuit crushing and screening - one stage closed circuit grinding - gravity separation - flotation (one coarse separation, two scavenging and three cleaning beneficiation) - concentrate dewatering process.
Ore: Gold
Capacity: 300-1000TPD
Process: Two stage one closed circuit crushing - one stage closed circuit grinding - one roughing, one scavenging, one cleaning and magnetic separation - fine tailings dehydration process.
Ore: Gold
Capacity: 300-1000TPD
Process: Two and a half closed circuit crushing and screening - one stage one closed circuit grinding and classification - one roughing, two scavenging and two fine flotation - concentrate dewatering process.
Ore: Gold
Capacity: 300-1000TPD
Process: Two stage closed-circuit crushing- Two stage closed-circuit grinding-All-slime cyanidation-Tailings dewatering
Ore: Copper
Capacity: 1000-3000TPD
Process: Two stages and one closed circuit crushing and screening-one stage of closed circuit grinding-copper flotation (one roughing, three scavenging and three concentration)-sulfur flotation (one roughing, two scavenging and three concentration)-concentrate dehydration-tailings dehydration process.
Ore: Gold
Capacity: 300-1000TPD
Process: Two-stage semi-closed circuit crushing and screening- two-stage closed circuit grinding and classifying- gravity separation-flotation separation-concentrate tailings dewatering process.
Ore: Tailings
Capacity: 300-1000TPD
Process: Gold Tailings Dry Stacking
Ore: Gold
Capacity: <300TPD
Process: Two-stage closed-circuit crushing--stage grinding--two roughing, three scavenging, and three cleaning--concentrate dewatering process.
Ore: Quartz Sand
Capacity: 300-1000TPD
Process: One-stage open-circuit self-grinding + one-stage closed-circuit grinding and classification + two-stage magnetic separation + one-stagedesliming + four-stage scrubbing - desliming + one-stage closed-circuitre grinding+ silicon powder dewatering + secondary fine powder dewatering process.
Ore: Gold
Capacity: 300-1000TPD
Process: Two stages, one closed circuit crushing and screening-one stage of closed circuit grinding-one roughing, two scavenging, and two fine flotation processes-two stages of mechanized dehydration process.
Ore: Gold
Capacity: 300-1000TPD
Process: Two stages and one closed circuit crushing and screening + one stage closed circuit grinding + flotation (one roughing, two scavenging and two concentration) + concentrate dewatering.