Ore: Feldspar
Capacity: 300-1000TPD
Process: Two-stage semi-closed-circuit crushing and screening process---One stage closed-circuit grinding and classifying process---One roughing three concentration three sweeping flotation process---Concentrate tailings conveying process
Ore: Lead-Zinc
Capacity: 1000-3000TPD
Process: Two-and-half-stage and one closed-circuit crushing and screening-One stage of grinding and grading-Flotation- Concentrated tailings dehydration process.
Ore: Tailings
Capacity: 1000-3000TPD
Process: The dehydration process of hydrocyclone + dehydration screen + filter press.
Ore: Phosphorite
Capacity: 1000-3000TPD
Process: Pre-screening and one-stage open-circuit crushing--one-stage grinding--three-stage reverse flotation--phosphate concentrate concentration and dewatering process.
Ore: Lead-Zinc
Capacity: 1000-3000TPD
Process: Two-and-half-stage and one closed-circuit crushing and screening+First closed-circuit grinding+ Zinc-sulfur bulk flotation+ Zinc-sulfur separation flotation+ Concentrate dehydration + Tailings dehydration process.
Ore: Lead-Zinc
Capacity: 1000-3000TPD
Process: Two and half stage closed-circuit crushing and screening – Three stage closed-circuit grinding- Lead flotation- Zinc flotation- Sulfur flotation-lead and zinc concentrate dewatering.
Ore: Multi-Metal
Capacity: 1000-3000TPD
Process: Three stage and one closed circuit crushing and screening – two stage closed circuit grinding – SO2 manganese leaching - cyanidation leaching silver in full wet process.
Ore: Fluorite
Capacity: 300-1000TPD
Process: Two-stage and one closed-circuit crushing and screening-First full closed-circuit grinding(first grinding+second grading)-Desulfurization flotation-Fluorite flotation (one-roughing, two-scavenging, eight-concentration+concentration I re-grinding closed-circuit)-concentrate dehydration process.